Video Rating: 0 / 5

Cell Condition after 42 Minutes of Corporation Plates Aluminum no Alloy

Second using dissimiliar metals. This time I am using a Lye solution and the aluminum chromate (6063-t52 temper with protective coating). No audio…sorry.
Video Rating: 0 / 5

My fourth prototype for a gas-propellant gun. If you just want to skip to the shooting, go to about 3:20 Version 3: www.youtube.com version 3 w/ n2o: www.youtube.com Version 2: www.youtube.com Version 1: www.youtube.com

Test three using dissimiliar metals in an HHO production. This time I am using a KOH solution. A far amount of hydrogen gas is forming off the stainless steel but very little (visually) oxygen gas is forming on the aluminum chromate (6063-t52 temper with chromate finish). No audio…sorry.

Final dissimiliar metals in this series of videos. In this one I use a piece of general purpose aluminum (3003 temper)rather than the aluminum chromate. The electrolyte is KOH. Here we see some of the effects others have stated. No audio…sorry.

Used stainless steel as the cathode and aluminum chromate as the anode. Interesting results. Tap water and no added electrolyte.

This demonstration shows how to rectify voltage using only a piece of aluminum and an electrolyte. Does not use semiconductors!

So i am giving my best shot at this HHO production test. There are 2 ways to make hydrogen electrolysis and a chemical reaction. So I am going to try and use both, which would be controling the chemical reaction with electrolysis. I have absolutly no clue what i am doing… So input would be appreciated